Stress corrosion of glass fibre reinforced polymers for infrastructure applications
Paper
Khennane, Amar and Melchers, Robert. 2002. "Stress corrosion of glass fibre reinforced polymers for infrastructure applications." 41st Australasian Corrosion Association Inc Conference (ACA 2001): Corrosion and Prevention. Newcastle, Australia 18 - 21 Nov 2001 Melbourne, Australia.
| Paper/Presentation Title | Stress corrosion of glass fibre reinforced polymers for infrastructure applications |
|---|---|
| Presentation Type | Paper |
| Authors | Khennane, Amar (Author) and Melchers, Robert (Author) |
| Journal or Proceedings Title | Durability of Materials: Corrosion and Prevention: Proceedings of the 41st Australasian Corrosion Association Inc Conference (ACA 2001) |
| Corrosion and Materials | |
| Journal Citation | 27, pp. 5-8 |
| Number of Pages | 4 |
| Year | 2002 |
| Place of Publication | Melbourne, Australia |
| ISSN | 1326-1932 |
| 1446-6848 | |
| Conference/Event | 41st Australasian Corrosion Association Inc Conference (ACA 2001): Corrosion and Prevention |
| Event Details | 41st Australasian Corrosion Association Inc Conference (ACA 2001): Corrosion and Prevention Event Date 18 to end of 21 Nov 2001 Event Location Newcastle, Australia |
| Public Notes | ©2001 Australasian Corrosion Association Inc. Paper 24. |
| Byline Affiliations | Department of Agricultural, Civil and Environmental Engineering |
| University of Newcastle | |
| Institution of Origin | University of Southern Queensland |
Permalink -
https://research.usq.edu.au/item/q0651/stress-corrosion-of-glass-fibre-reinforced-polymers-for-infrastructure-applications
Download files
1759
total views219
total downloads5
views this month0
downloads this month