Monte-Carlo simulation of the durability of glass fibre reinforced composite under environmental stress corrosion

Paper


Nguyen-Van, Hieu, Khennane, Amar and Tran-Cong, Thanh. 2006. "Monte-Carlo simulation of the durability of glass fibre reinforced composite under environmental stress corrosion." Nguyen, Son Q. and Nguyen, Dung (ed.) 2006 International Conference on Nonlinear Analysis & Engineering Mechanics Today. Ho Chi Minh City, Vietnam 11 - 14 Dec 2006 Paris, France.
Paper/Presentation Title

Monte-Carlo simulation of the durability of glass fibre reinforced composite under environmental stress corrosion

Presentation TypePaper
AuthorsNguyen-Van, Hieu (Author), Khennane, Amar (Author) and Tran-Cong, Thanh (Author)
EditorsNguyen, Son Q. and Nguyen, Dung
Journal or Proceedings TitleProceedings of the 2006 International Conference on Nonlinear Analysis & Engineering Mechanics Today
Year2006
Place of PublicationParis, France
Web Address (URL) of Paperhttp://www.lms.polytechnique.fr/CONGRES/AN-EMT2006.html
Conference/Event2006 International Conference on Nonlinear Analysis & Engineering Mechanics Today
Event Details
2006 International Conference on Nonlinear Analysis & Engineering Mechanics Today
Event Date
11 to end of 14 Dec 2006
Event Location
Ho Chi Minh City, Vietnam
Abstract

The lifetime distribution of glass fibre subject to permanent environmental stress corrosion is very important for assessing the durability and damage tolerance of composites using glass reinforcement. A mechanical model based on the statistics of flaw spectra during stress corrosion and 3D shear lag model is presented. The proposed approach shows that it is possible to
identify the influence of stress corrosion properties on the long term durability of glass fibre reinforced composites (GFRP).

Keywordsglass fibre, reinforced composites
ANZSRC Field of Research 2020401799. Mechanical engineering not elsewhere classified
401602. Composite and hybrid materials
Byline AffiliationsComputational Engineering and Science Research Centre
Permalink -

https://research.usq.edu.au/item/9y0z7/monte-carlo-simulation-of-the-durability-of-glass-fibre-reinforced-composite-under-environmental-stress-corrosion

Download files

  • 2392
    total views
  • 724
    total downloads
  • 8
    views this month
  • 2
    downloads this month

Export as

Related outputs

A non-boundary-fitted-grid method, based on compact integrated-RBF approximations, for solving differential problems in multiply-connected domains
Le, T.T.V., Mai-Duy, N., Le-Cao, K., Bordas, S., Vu, D.P. and Tran-Cong, T.. 2024. "A non-boundary-fitted-grid method, based on compact integrated-RBF approximations, for solving differential problems in multiply-connected domains." Journal of Computational Science. 79. https://doi.org/10.1016/j.jocs.2024.102311
Limit state analysis of reinforced concrete slabs using an integrated radial basis function based mesh-free method
Ho, Phuc L. H., Le, Canh V. and Tran-Cong, T.. 2018. "Limit state analysis of reinforced concrete slabs using an integrated radial basis function based mesh-free method." Applied Mathematical Modelling: simulation and computation for engineering and environmental systems. 53, pp. 1-11. https://doi.org/10.1016/j.apm.2017.08.006
Coarse-graining, compressibility, and thermal fluctuation scaling in dissipative particle dynamics employed with pre-determined input parameters
Mai-Duy, N., Phan-Thien, N., Nguyen, T. Y. N. and Tran-Cong, T.. 2020. "Coarse-graining, compressibility, and thermal fluctuation scaling in dissipative particle dynamics employed with pre-determined input parameters." Physics of Fluids. 32 (5). https://doi.org/10.1063/5.0010275
A time discretization scheme based on integrated radial basis functions for heat transfer and fluid flow problems
Le, T. T. V., Mai-Duy, N., Le-Cao, K. and Tran-Cong, T.. 2018. "A time discretization scheme based on integrated radial basis functions for heat transfer and fluid flow problems." Numerical Heat Transfer Part B: Fundamentals. 74 (2), pp. 498-518. https://doi.org/10.1080/10407790.2018.1515329
A symmetric integrated radial basis function method for solving differential equations
Mai-Duy, Nam, Dalal, Deepak, Le, Thi Thuy Van, Ngo-Cong, Duc and Tran-Cong, Thanh. 2018. "A symmetric integrated radial basis function method for solving differential equations." Numerical Methods for Partial Differential Equations. 34 (3), pp. 959-981. https://doi.org/10.1002/num.22240
Isotropic turbulence surpasses gravity in affecting bubble-particle collision interaction in flotation
Ngo-Cong, Duc, Nguyen, Anh V. and Tran-Cong, Thanh. 2018. "Isotropic turbulence surpasses gravity in affecting bubble-particle collision interaction in flotation." Minerals Engineering. 122, pp. 165-175. https://doi.org/10.1016/j.mineng.2018.03.033
Predicting water allocation trade prices using a hybrid Artificial Neural Network-Bayesian modelling approach
Nguyen-Ky, Tai, Mushtaq, Shahbaz, Loch, Adam, Reardon-Smith, Kate, An-Vo, Duc-Anh, Ngo-Cong, Duc and Tran-Cong, Thanh. 2018. "Predicting water allocation trade prices using a hybrid Artificial Neural Network-Bayesian modelling approach." Journal of Hydrology. 567, pp. 781-791. https://doi.org/10.1016/j.jhydrol.2017.11.049
A generalised finite difference scheme based on compact integrated radial basis function for flow in heterogeneous soils
Ngo-Cong, D., Tien, C.M.T., Nguyen-Ky, T., An-Vo, D.-A., Mai-Duy, N., Strunin, D. V. and Tran-Cong, T.. 2017. "A generalised finite difference scheme based on compact integrated radial basis function for flow in heterogeneous soils." International Journal for Numerical Methods in Fluids. 85 (7), pp. 404-429. https://doi.org/10.1002/fld.4386
Imposition of physical parameters in dissipative particle dynamics
Mai-Duy, N., Phan-Thien, N. and Tran-Cong, T.. 2017. "Imposition of physical parameters in dissipative particle dynamics." Computer Physics Communications. 221, pp. 290-298. https://doi.org/10.1016/j.cpc.2017.09.003
A numerical study of compact approximations based on flat integrated radial basis functions for second-order differential equations
Tien, C. M. T., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2016. "A numerical study of compact approximations based on flat integrated radial basis functions for second-order differential equations." Computers and Mathematics with Applications. 72 (9), pp. 2364-2387. https://doi.org/10.1016/j.camwa.2016.09.001
High-order fluid solver based on a combined compact integrated RBF approximation and its fluid structure interaction applications
Tien, C. M. T, Ngo-Cong, D., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2016. "High-order fluid solver based on a combined compact integrated RBF approximation and its fluid structure interaction applications." Computers and Fluids. 131, pp. 151-168. https://doi.org/10.1016/j.compfluid.2016.03.021
An improved dissipative particle dynamics scheme
Mai-Duy, N., Phan-Thien, N. and Tran-Cong, T.. 2017. "An improved dissipative particle dynamics scheme." Applied Mathematical Modelling: simulation and computation for engineering and environmental systems. 46, pp. 602-617. https://doi.org/10.1016/j.apm.2017.01.086
Compact approximation stencils based on integrated flat radial basis functions
Mai-Duy, N., Le, T. T. V., Tien, C. M. T., Ngo-Cong, D. and Tran-Cong, T.. 2017. "Compact approximation stencils based on integrated flat radial basis functions." Engineering Analysis with Boundary Elements. 74, pp. 79-87. https://doi.org/10.1016/j.enganabound.2016.11.002
Displacement and equilibrium mesh-free formulation based on integrated radial basis functions for dual yield design
Ho, Phuc L. H., Le, Canh V. and Tran-Cong, Thanh. 2016. "Displacement and equilibrium mesh-free formulation based on integrated radial basis functions for dual yield design." Engineering Analysis with Boundary Elements. 71, pp. 92-100. https://doi.org/10.1016/j.enganabound.2016.07.010
A review of stochastic description of the turbulence effect on bubble-particle interactions in flotation
Nguyen, Anh V., An-Vo, Duc-Anh, Tran-Cong, Thanh and Evans, Geoffrey M.. 2016. "A review of stochastic description of the turbulence effect on bubble-particle interactions in flotation." International Journal of Mineral Processing. 156, pp. 75-86. https://doi.org/10.1016/j.minpro.2016.05.002
RBFN stochastic coarse-grained simulation method: Part I - Dilute polymer solutions using bead-spring chain models
Nguyen, H. Q., Tran, C.-D. and Tran-Cong, T.. 2015. "RBFN stochastic coarse-grained simulation method: Part I - Dilute polymer solutions using bead-spring chain models." CMES Computer Modeling in Engineering and Sciences. 105 (5), pp. 399-439. https://doi.org/10.3970/cmes.2015.105.399
A three-point coupled compact integrated RBF scheme for second-order differential problems
Tien, C. M. T., Thai-Quang, N., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2015. "A three-point coupled compact integrated RBF scheme for second-order differential problems." CMES Computer Modeling in Engineering and Sciences. 104 (6), pp. 425-469. https://doi.org/10.3970/cmes.2015.104.425
Simulation of flow of fibre suspensions using an IRBF-BCF based multiscale approach
Nguyen, H. Q., Tran, C.-D. and Tran-Cong, T.. 2015. "Simulation of flow of fibre suspensions using an IRBF-BCF based multiscale approach." Solnordal, C. B., Liovic, P., Delaney, G. W., Cummins, S. J., Schwarz, M. P. and Witt, P. J. (ed.) 11th International Conference on Computational Fluid Dynamics in the Minerals and Process Industries (CFD2015). Melbourne, Australia 07 - 09 Dec 2015 Australia.
Stable integrated RBF calculation using preconditioning and high-order compact approximation for second-order PDEs
Tien, C. M. T., Mai-Duy, N., Ngo-Cong, D., Tran, C. D. and Tran-Cong, T.. 2015. "Stable integrated RBF calculation using preconditioning and high-order compact approximation for second-order PDEs." Witt, Peter (ed.) Eleventh International Conference on Computational Fluid Dynamics in the Minerals and Process Industries 2015. Melbourne, Victoria 07 - 09 Dec 2015 Australia.
Incompressible smoothed particle hydrodynamics-moving IRBFN method for viscous flow problems
Ngo-Cong, D., Tran, C.-D., Mai-Duy, N. and Tran-Cong, T.. 2015. "Incompressible smoothed particle hydrodynamics-moving IRBFN method for viscous flow problems." Engineering Analysis with Boundary Elements. 59, pp. 172-186. https://doi.org/10.1016/j.enganabound.2015.06.006
Improving rockbolt design in tunnels using topology optimisation
Nguyen, Tin, Ghabraie, Kazem, Tran-Cong, Thanh and Fatahi, Behzad. 2016. "Improving rockbolt design in tunnels using topology optimisation." International Journal of Geomechanics. 16 (1). https://doi.org/10.1061/(ASCE)GM.1943-5622.0000488
High-order fully coupled scheme based on compact integrated RBF approximation for viscous flows in regular and irregular domains
Tien, C. M. T., Thai-Quang, N., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2015. "High-order fully coupled scheme based on compact integrated RBF approximation for viscous flows in regular and irregular domains." CMES Computer Modeling in Engineering and Sciences. 105 (4), pp. 301-340. https://doi.org/10.3970/cmes.2015.105.301
A multiscale method based on the fibre configuration field, IRBF and DAVSS for the simulation of fibre suspension flows
Nguyen, H. Q., Tran, C.-D. and Tran-Cong, T.. 2015. "A multiscale method based on the fibre configuration field, IRBF and DAVSS for the simulation of fibre suspension flows." CMES: Computer Modeling in Engineering and Science. 109 (4), pp. 361-403. https://doi.org/10.3970/cmes.2015.109.361
A high-order coupled compact integrated RBF approximation based domain decomposition algorithm for second-order differential problems
Tien, C. M. T., Pham-Sy, N., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2015. "A high-order coupled compact integrated RBF approximation based domain decomposition algorithm for second-order differential problems." CMES Computer Modeling in Engineering and Sciences. 104 (4), pp. 251-304. https://doi.org/10.3970/cmes.2015.104.251
Nonlinear Optimisation Using Production Functions to Estimate Economic Benefit of Conjunctive Water Use for Multicrop Production
An-Vo, D.-A., Mushtaq, S., Nguyen-Ky, T., Bundschuh, J., Tran-Cong, T., Maraseni, T. N. and Reardon-Smith, K.. 2015. "Nonlinear Optimisation Using Production Functions to Estimate Economic Benefit of Conjunctive Water Use for Multicrop Production." Water Resources Management. 29 (7), pp. 2153-2170. https://doi.org/10.1007/s11269-015-0933-y
Higher-order approximation of contaminant transport equation for turbulent channel flows based on centre manifolds and its numerical solution
Ngo-Cong, D., Mohammed, F. J., Strunin, D. V., Skvortsov, A. T., Mai-Duy, N. and Tran-Cong, T.. 2015. "Higher-order approximation of contaminant transport equation for turbulent channel flows based on centre manifolds and its numerical solution." Journal of Hydrology. 525, pp. 87-101. https://doi.org/10.1016/j.jhydrol.2015.03.038
Large deflection analysis of plates and cylindrical shells by an efficient four-node flat element with mesh distortions
Nguyen-Van, H., Nguyen-Hoai, N., Chau-Dinh, T. and Tran-Cong, T.. 2015. "Large deflection analysis of plates and cylindrical shells by an efficient four-node flat element with mesh distortions." Acta Mechanica. 226 (8), pp. 2693-2713. https://doi.org/10.1007/s00707-015-1339-x
Parallel control-volume method based on compact local integrated RBFs for the solution of fluid flow problems
Pham-Sy, N., Tran, C.-D., Mai-Duy, N. and Tran-Cong, T.. 2014. "Parallel control-volume method based on compact local integrated RBFs for the solution of fluid flow problems." CMES Computer Modeling in Engineering and Sciences. 100 (5), pp. 363-397. https://doi.org/10.3970/cmes.2014.100.363
Geopolymer concrete-filled pultruded composite beams: concrete mix design and application
Ferdous, Wahid, Manalo, Allan, Khennane, Amar and Kayali, Obada. 2015. "Geopolymer concrete-filled pultruded composite beams: concrete mix design and application." Cement and Concrete Composites. 58, pp. 1-13. https://doi.org/10.1016/j.cemconcomp.2014.12.012
Simultaneous pattern and size optimisation of rock bolts for underground excavations
Nguyen, Tin, Ghabraie, Kazem and Tran-Cong, Thanh. 2015. "Simultaneous pattern and size optimisation of rock bolts for underground excavations." Computers and Geotechnics. 66, pp. 264-277. https://doi.org/10.1016/j.compgeo.2015.02.007
Asymptotics of averaged turbulent transfer in canopy flows
Mohammed, F. J., Strunin, D. V., Ngo-Cong, D. and Tran-Cong, T.. 2015. "Asymptotics of averaged turbulent transfer in canopy flows." Journal of Engineering Mathematics. 91 (1), pp. 81-104. https://doi.org/10.1007/s10665-014-9737-y
A meshless numerical approach based on integrated radial basis functions and level set method for interfacial flows
Mai-Cao, L. and Tran-Cong, T.. 2014. "A meshless numerical approach based on integrated radial basis functions and level set method for interfacial flows ." Applied Mathematical Modelling: simulation and computation for engineering and environmental systems. 38 (23), pp. 5743-5766. https://doi.org/10.1016/j.apm.2014.06.018
A fully coupled scheme for viscous flows in regular and irregular domains using compact integrated RBF approximation
Tien, C. M. T., Thai-Quang, N., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2014. "A fully coupled scheme for viscous flows in regular and irregular domains using compact integrated RBF approximation." Applied Mechanics and Materials. 553, pp. 138-143. https://doi.org/10.4028/www.scientific.net/AMM.553.138
A numerical solution based on the Fokker-Planck equation for dilute polymer solutions using high order RBF methods
Nguyen, H. Q., Tran, C.-D., Pham-Sy, N. and Tran-Cong, T.. 2014. "A numerical solution based on the Fokker-Planck equation for dilute polymer solutions using high order RBF methods." Applied Mechanics and Materials. 553, pp. 187-192. https://doi.org/10.4028/www.scientific.net/AMM.553.187
Modelling dispersion in laminar and turbulent flows in an open channel based on centre manifolds using 1D-IRBFN method
Mohammed, F. J., Ngo-Cong, D., Strunin, D. V., Mai-Duy, N. and Tran-Cong, T.. 2014. "Modelling dispersion in laminar and turbulent flows in an open channel based on centre manifolds using 1D-IRBFN method." Applied Mathematical Modelling: simulation and computation for engineering and environmental systems. 38 (14), pp. 3672-3691. https://doi.org/10.1016/j.apm.2013.12.007
Benefits of geopolymer concrete-filled FRP beams and its flexural behaviour
Ferdous, Wahid, Manalo, Allan, Khennane, Amar and Kayali, Obada. 2014. "Benefits of geopolymer concrete-filled FRP beams and its flexural behaviour." Australasian Composites Conference (CA 2014): Materials for a Lighter and Smarter World. Newcastle, Australia 07 - 09 Apr 2014 Melbourne, Australia.
A compact five-point stencil based on integrated RBFs for 2D second-order differential problems
Mai-Duy, N. and Tran-Cong, T.. 2013. "A compact five-point stencil based on integrated RBFs for 2D second-order differential problems." Journal of Computational Physics. 235, pp. 302-321. https://doi.org/10.1016/j.jcp.2012.10.048
Modelling of solid bodies in dissipative particle dynamics
Mai-Duy, N., Phan-Thien, N., Khoo, B. C. and Tran-Cong, T.. 2013. "Modelling of solid bodies in dissipative particle dynamics." Bischoff, M., Onate, E., Owen, D. R. J., Ramm, E. and Wriggers, P. (ed.) 3rd International Conference on Particle-based Methods Fundamentals and Applications (Particles 2013): Particle-Based Methods III: Fundamentals and Applications. Stuttgart, Germany 18 - 20 Sep 2013 Barcelona, Spain.
ADI method based on C2-continuous two-node integrated-RBF elements for viscous flows
An-Vo, D.-A., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2013. "ADI method based on C2-continuous two-node integrated-RBF elements for viscous flows." Applied Mathematical Modelling: simulation and computation for engineering and environmental systems. 37 (7), pp. 5184-5203. https://doi.org/10.1016/j.apm.2012.10.034
A direct forcing immersed boundary method employed with compact integrated RBF approximations for heat transfer and fluid flow problems
Thai-Quang, N., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2013. "A direct forcing immersed boundary method employed with compact integrated RBF approximations for heat transfer and fluid flow problems." CMES Computer Modeling in Engineering and Sciences. 96 (1), pp. 49-90. https://doi.org/10.3970/cmes.2013.096.049
Compact local IRBF and domain decomposition method for solving PDEs using a distributed termination detection based parallel algorithm
Pham-Sy, N., Tran, C.-D., Hoang-Trieu, T.-T., Mai-Duy, N. and Tran-Cong, T.. 2013. "Compact local IRBF and domain decomposition method for solving PDEs using a distributed termination detection based parallel algorithm." CMES Computer Modeling in Engineering and Sciences. 92 (1), pp. 1-31. https://doi.org/10.3970/cmes.2013.092.001
A finite-volume method based on compact local integrated radial basis function approximations for second-order differential problems
Hoang-Trieu, T.-T., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2013. "A finite-volume method based on compact local integrated radial basis function approximations for second-order differential problems." CMES Computer Modeling in Engineering and Sciences. 91 (6), pp. 485-516. https://doi.org/10.3970/cmes.2013.091.485
A numerical scheme based on compact integrated-RBFs and Adams-Bashforth/Crank-Nicolson algorithms for diffusion and unsteady fluid flow problems
Thai-Quang, N., Le-Cao, K., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2013. "A numerical scheme based on compact integrated-RBFs and Adams-Bashforth/Crank-Nicolson algorithms for diffusion and unsteady fluid flow problems." Engineering Analysis with Boundary Elements. 37 (12), pp. 1653-1667. https://doi.org/10.1016/j.enganabound.2013.09.011
A compact 9 point stencil based on integrated RBFs for the convection-diffusion equation
Mai-Duy, N., Thai-Quang, N., Hoang-Trieu, T.-T. and Tran-Cong, T.. 2014. "A compact 9 point stencil based on integrated RBFs for the convection-diffusion equation." Applied Mathematical Modelling: simulation and computation for engineering and environmental systems. 38 (4), pp. 1495-1510. https://doi.org/10.1016/j.apm.2013.08.017
Applying bi-directional evolutionary structural optimisation method for tunnel reinforcement design considering nonlinear material behaviour
Nguyen, T., Ghabraie, K. and Tran-Cong, T.. 2014. "Applying bi-directional evolutionary structural optimisation method for tunnel reinforcement design considering nonlinear material behaviour." Computers and Geotechnics. 55, pp. 57-66. https://doi.org/10.1016/j.compgeo.2013.07.015
Simulation of Newtonian-fluid flows with C2-continuous two-node integrated-RBF elements
An-Vo, D.-A., Mai-Duy, N. and Tran-Cong, T.. 2010. "Simulation of Newtonian-fluid flows with C2-continuous two-node integrated-RBF elements." Structural Longevity. 4 (1), pp. 39-45. https://doi.org/10.3970/sl.2010.004.039
Compact local stencils employed with integrated RBFs for fourth-order differential problems
Hoang-Trieu, T.-T., Mai-Duy, N. and Tran-Cong, T.. 2011. "Compact local stencils employed with integrated RBFs for fourth-order differential problems." Structural Longevity. 6 (2), pp. 93-107. https://doi.org/10.3970/sl.2011.006.093
A numerical study of integrated radial-basis-functions for the pressure-velocity formulation
Thai-Quang, Nha, Mai-Duy, Nam and Tran-Cong, Thanh. 2012. "A numerical study of integrated radial-basis-functions for the pressure-velocity formulation." 7th ICCES Special Symposium on Meshless & Other Novel Computational Methods (ICCES MM 2011). Zonguldak, Turkey 06 - 10 Sep 2011 USA.
RBF computation of multiscale elliptic problems [Keynote paper]
An-Vo, D.-A., Tran, C.-D., Mai-Duy, N. and Tran-Cong, T.. 2012. "RBF computation of multiscale elliptic problems [Keynote paper]." Atluri, S. N., Vusanovic, I. and Sarler, B. (ed.) 8th ICCES Special Symposium on Meshless & Other Novel Computational Methods (ICCES MM 2012). Budva, Montenegro 02 - 06 Sep 2012 Montenegro.
Discretisation of the velocity-pressure formulation with integrated radial-basis-function networks
Thai-Quang, N., Le-Cao, K., Mai-Duy, N. and Tran-Cong, T.. 2011. "Discretisation of the velocity-pressure formulation with integrated radial-basis-function networks." Structural Longevity. 6 (2), pp. 77-91. https://doi.org/10.3970/sl.2011.006.077
Computation of a Fokker-Planck-equation-based multi-scale model for complex flows using the IRBFN method
Tran, Canh-Dung, Mai-Duy, Nam and Tran-Cong, Thanh. 2012. "Computation of a Fokker-Planck-equation-based multi-scale model for complex flows using the IRBFN method." Eberhardsteiner, J., Böhm, H. J. and Rammerstorfer, F. G. (ed.) 6th European Congress on Computational Methods in Applied Sciences and Engineering (ECCOMAS 2012). Vienna, Austria Vienna, Austria.
Numerical solution of Fokker-Planck equation using the integral radial basis function networks
Tran, C.-D., Mai-Duy, N. and Tran-Cong, T.. 2012. "Numerical solution of Fokker-Planck equation using the integral radial basis function networks." Pimenta, P. M. and Campello, E. M. B. (ed.) 10th World Congress on Computational Mechanics (WCCM 2012). Sao Paulo, Brazil 08 - 13 Jul 2012 Sao Paulo, Brazil. https://doi.org/10.5151/10.5151/meceng-wccm2012-19433
Modeling strain localisation in a segmented bar by a C2-continuous two-node integrated-RBF element formulation
An-Vo, D.-A., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2012. "Modeling strain localisation in a segmented bar by a C2-continuous two-node integrated-RBF element formulation." Brebbia, C. A. and Poljak, D. (ed.) 34th International Conference on Boundary Elements and other Mesh Reduction Methods (BEM/MRM 2012). Split, Croatia 25 - 27 Jun 2012 United Kingdom. https://doi.org/10.2495/BE120011
A new IRBFN scheme for the numerical simulation of interfacial flows
Mai-Cao, L. and Tran-Cong, T.. 2012. "A new IRBFN scheme for the numerical simulation of interfacial flows." Gu, Y. T. and Saha, Suvash C. (ed.) 4th International Conference on Computational Methods (ICCM 2012). Gold Coast, Australia 25 - 28 Nov 2012 Brisbane, Australia.
Development of parallel algorithm for boundary value problems using compact local integrated RBFN and domain decomposition
Pham-Sy, N., Hoang-Trieu, T.-T., Tran, C.-D., Mai-Duy, N. and Tran-Cong, T.. 2012. "Development of parallel algorithm for boundary value problems using compact local integrated RBFN and domain decomposition." Gu, Y. T. and Saha, Suvash C. (ed.) 4th International Conference on Computational Methods (ICCM 2012). Gold Coast, Australia 25 - 28 Nov 2012 Brisbane, Australia.
A high-order compact integrated-RBF scheme for time-dependent problems
Thai-Quang, N., Le-Cao, K., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2012. "A high-order compact integrated-RBF scheme for time-dependent problems." Gu, Y. T. and Saha, Suvash C. (ed.) 4th International Conference on Computational Methods (ICCM 2012). Gold Coast, Australia 25 - 28 Nov 2012 Brisbane, Australia.
Compact local integrated RBF stencil based on finite volume formulation for second-order differential problems
Hoang-Trieu, T.-T., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2012. "Compact local integrated RBF stencil based on finite volume formulation for second-order differential problems." Gu, Y. T. and Saha, Suvash C. (ed.) 4th International Conference on Computational Methods (ICCM 2012). Gold Coast, Australia 25 - 28 Nov 2012 Brisbane, Australia.
High-order alternating direction implicit method based on compact integrated-RBF approximations for unsteady/steady convection-diffusion equations
Thai-Quang, N., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2012. "High-order alternating direction implicit method based on compact integrated-RBF approximations for unsteady/steady convection-diffusion equations." CMES Computer Modeling in Engineering and Sciences. 89 (3), pp. 189-220. https://doi.org/10.3970/cmes.2012.089.189
RBF-based multiscale control volume method for second order elliptic problems with oscillatory coefficients
An-Vo, D.-A., Tran, C.-D., Mai-Duy, N. and Tran-Cong, T.. 2012. "RBF-based multiscale control volume method for second order elliptic problems with oscillatory coefficients." CMES Computer Modeling in Engineering and Sciences. 89 (4), pp. 303-359. https://doi.org/10.3970/cmes.2012.089.303
Local Moving Least Square - One-Dimensional IRBFN Technique: Part II- Unsteady Incompressible Viscous Flows
Ngo-Cong, D., Mai-Duy, N., Karunasena, W. and Tran-Cong, T.. 2012. "Local Moving Least Square - One-Dimensional IRBFN Technique: Part II- Unsteady Incompressible Viscous Flows ." CMES Computer Modeling in Engineering and Sciences. 83 (3), pp. 311-351. https://doi.org/10.3970/cmes.2012.083.311
Local Moving Least Square - One-Dimensional IRBFN Technique: Part I - Natural Convection Flows in Concentric and Eccentric Annuli
Ngo-Cong, D., Mai-Duy, N., Karunasena, W. and Tran-Cong, T.. 2012. "Local Moving Least Square - One-Dimensional IRBFN Technique: Part I - Natural Convection Flows in Concentric and Eccentric Annuli ." CMES Computer Modeling in Engineering and Sciences. 83 (3), pp. 275-310. https://doi.org/10.3970/cmes.2012.083.275
A continuum-microscopic method based on IRBFs and control volume scheme for viscoelastic fluid flows
Tran, C.-D., Mai-Duy, N., Le-Cao, K. and Tran-Cong, T.. 2012. "A continuum-microscopic method based on IRBFs and control volume scheme for viscoelastic fluid flows." CMES Computer Modeling in Engineering and Sciences. 85 (6), pp. 499-519. https://doi.org/10.3970/cmes.2012.085.499
Processing the CNTs' interaction in web using an electro-static field based process
Tran, Canh-Dung, Tran-Cong, Thanh, Le-Cao, K. and Ho-Minh, D.. 2012. "Processing the CNTs' interaction in web using an electro-static field based process." Griffin, Brendan, Faraone, Lorenzo and Martyniuk, Mariusz (ed.) 2012 International Conference on Nanoscience and Nanotechnology (ICONN 2012). Perth, Australia 05 - 09 Feb 2012 Piscataway, NJ. United States.
Tunnel reinforcement optimisation for nonlinear material
Nguyen, T., Ghabraie, K. and Tran-Cong, T.. 2012. "Tunnel reinforcement optimisation for nonlinear material." Gu, Y. T. and Saha, Suvash C. (ed.) 4th International Conference on Computational Methods (ICCM 2012). Gold Coast, Australia 25 - 28 Nov 2012 Brisbane, Australia.
A high-order compact local integrated-RBF scheme for steady-state incompressible viscous flows in the primitive variables
Thai-Quang, N., Le-Cao, K., Mai-Duy, N. and Tran-Cong, T.. 2012. "A high-order compact local integrated-RBF scheme for steady-state incompressible viscous flows in the primitive variables." CMES Computer Modeling in Engineering and Sciences. 84 (6), pp. 528-557. https://doi.org/10.3970/cmes.2012.084.528
A numerical procedure based on 1D-IRBFN and local MLS-1D-IRBFN methods for fluid-structure interaction analysis
Ngo-Cong, D., Mai-Duy, N., Karunasena, W. and Tran-Cong, T.. 2012. "A numerical procedure based on 1D-IRBFN and local MLS-1D-IRBFN methods for fluid-structure interaction analysis." CMES Computer Modeling in Engineering and Sciences. 83 (5), pp. 459-498. https://doi.org/10.3970/cmes.2012.083.459
Local moving least square-one-dimensional integrated radial basis function networks technique for incompressible viscous flows
Ngo-Cong, D., Mai-Duy, N., Karunasena, W. and Tran-Cong, T.. 2012. "Local moving least square-one-dimensional integrated radial basis function networks technique for incompressible viscous flows." International Journal for Numerical Methods in Fluids. 70 (11), pp. 1443-1474. https://doi.org/10.1002/fld.3640
Several compact local stencils based on integrated RBFs for fourth-order ODEs and PDEs
Hoang-Trieu, T.-T., Mai-Duy, N. and Tran-Cong, T.. 2012. "Several compact local stencils based on integrated RBFs for fourth-order ODEs and PDEs." CMES Computer Modeling in Engineering and Sciences. 84 (2), pp. 171-203. https://doi.org/10.3970/cmes.2012.084.171
Simulation of viscous and viscoelastic flows using a RBF-Galerkin approach
Ho-Minh, D., Mai-Duy, N. and Tran-Cong, T.. 2012. "Simulation of viscous and viscoelastic flows using a RBF-Galerkin approach." Australian Journal of Mechanical Engineering. 9 (2), pp. 101-112. https://doi.org/10.7158/M10-719.2012.9.2
Moving least square: one dimensional integrated radial basis function networks for time dependent problems
Ngo-Cong, D., Mai-Duy, N., Karunasena, W. and Tran-Cong, T.. 2011. "Moving least square: one dimensional integrated radial basis function networks for time dependent problems." Brebbia, C. A. and Popov, V. (ed.) 33rd International Conference on Boundary Elements and other Mesh Reduction Methods (BEM/MRM 2011). New Forest, United Kingdom 28 - 30 Jun 2011 Southampton, UK. https://doi.org/10.2495/BE110271
IRBFN-based multiscale solution of a model 1D elliptic equation
An-Vo, D.-A., Tran, C.-D., Mai-Duy, N. and Tran-Cong, T.. 2011. "IRBFN-based multiscale solution of a model 1D elliptic equation." Brebbia, C. A. and Popov, V. (ed.) 33rd International Conference on Boundary Elements and other Mesh Reduction Methods (BEM/MRM 2011). New Forest, United Kingdom 28 - 30 Jun 2011 Southampton, United Kingdom. https://doi.org/10.2495/BE110211
Numerical study of stream-function formulation governing flows in multiply-connected domains by integrated RBFs and Cartesian grids
Le-Cao, K., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2011. "Numerical study of stream-function formulation governing flows in multiply-connected domains by integrated RBFs and Cartesian grids." Computers and Fluids. 44 (1), pp. 32-42. https://doi.org/10.1016/j.compfluid.2010.11.027
An integrated RBFN-based macro-micro multi-scale method for computation of visco-elastic fluid flows
Tran, C.-D., An-Vo, D.-A., Mai-Duy, N. and Tran-Cong, T.. 2011. "An integrated RBFN-based macro-micro multi-scale method for computation of visco-elastic fluid flows." CMES Computer Modeling in Engineering and Sciences. 82 (2), pp. 137-162. https://doi.org/10.3970/cmes.2011.082.137
Manufacturing polymer/carbon nanotube composite using a novel direct process
Tran, C.-D., Lucas, S., Phillips, D. G., Randeniya, L. K., Baughman, R. H. and Tran-Cong, T.. 2011. "Manufacturing polymer/carbon nanotube composite using a novel direct process." Nanotechnology. 22 (14), pp. 1453021-1453029. https://doi.org/10.1088/0957-4484/22/14/145302
Compact local approximations employed with integrated RBFs for second-order elliptic differential equations
Mai-Duy, Nam and Tran-Cong, Thanh. 2011. "Compact local approximations employed with integrated RBFs for second-order elliptic differential equations." Yang, Yeong-Bin, Leu, Liang-Jenq and Chen, Chuin-Shan David (ed.) 3rd International Symposium on Computational Mechanics (ISCM III) and 2nd Symposium on Computational Structural Engineering (CSE II). Taipei, Taiwan 05 - 07 Dec 2011 Taiwan.
A stable and accurate control-volume technique based on integrated radial basis function networks for fluid-flow problems
Mai-Duy, N. and Tran-Cong, T.. 2011. "A stable and accurate control-volume technique based on integrated radial basis function networks for fluid-flow problems." Teh, Kian, Davies, Ian and Howard, Ian (ed.) 6th Australasian Congress on Applied Mechanics (ACAM 6). Perth, Western Australia 12 - 15 Dec 2010 Perth, Western Australia. Taylor & Francis. https://doi.org/10.1080/14484846.2011.11464606
A numerical technique based on integrated RBFs for the system evolution in molecular dynamics
Mai-Duy, N., Tran-Cong, T. and Phan-Thien, N.. 2011. "A numerical technique based on integrated RBFs for the system evolution in molecular dynamics." CMES Computer Modeling in Engineering and Sciences. 79 (4), pp. 223-236. https://doi.org/10.3970/cmes.2011.079.223
High-order upwind methods based on C2-continuous two-node integrated-RBF elements for viscous flows
An-Vo, D. A., Mai-Duy, N. and Tran-Cong, T.. 2011. "High-order upwind methods based on C2-continuous two-node integrated-RBF elements for viscous flows." CMES Computer Modeling in Engineering and Sciences. 80 (2), pp. 141-177. https://doi.org/10.3970/cmes.2011.080.141
A C2-continuous control-volume technique based on cartesian grids and two-node integrated-RBF elements for second-order elliptic problems
An-Vo, D. A., Mai-Duy, N. and Tran-Cong, T.. 2011. "A C2-continuous control-volume technique based on cartesian grids and two-node integrated-RBF elements for second-order elliptic problems." CMES Computer Modeling in Engineering and Sciences. 72 (4), pp. 299-334. https://doi.org/10.3970/cmes.2011.072.299
Buckling and vibration analysis of laminated composite plate/shell structures via a smoothed quadrilateral flat shell element with in-plane rotations
Nguyen-Van, H., Mai-Duy, N., Karunasena, W. and Tran-Cong, T.. 2011. "Buckling and vibration analysis of laminated composite plate/shell structures via a smoothed quadrilateral flat shell element with in-plane rotations." Computers and Structures. 89 (7-8), pp. 612-625. https://doi.org/10.1016/j.compstruc.2011.01.005
Free vibration analysis of laminated composite plates based on FSDT using one-dimensional IRBFN method
Ngo-Cong, D., Mai-Duy, N., Karunasena, W. and Tran-Cong, T.. 2011. "Free vibration analysis of laminated composite plates based on FSDT using one-dimensional IRBFN method." Computers and Structures. 89 (1-2), pp. 1-13. https://doi.org/10.1016/j.compstruc.2010.07.012
A high-order upwind control-volume method based on integrated RBFs for fluid-flow problems
Mai-Duy, N. and Tran-Cong, T.. 2011. "A high-order upwind control-volume method based on integrated RBFs for fluid-flow problems." International Journal for Numerical Methods in Fluids. 67 (12), pp. 1973-1992. https://doi.org/10.1002/fld.2477
Crack identification in reinforced concrete beams using ANSYS software
Dahmani, L., Khennane, A. and Kaci, S.. 2010. "Crack identification in reinforced concrete beams using ANSYS software ." Strength of Materials. 42 (2), pp. 232-240. https://doi.org/10.1007/s11223-010-9212-6
Development and application of assumed strain smoothing finite element technique for composite plate/shell structures
Nguyen-Van, Hieu. 2009. Development and application of assumed strain smoothing finite element technique for composite plate/shell structures. PhD Thesis Doctor of Philosophy. University of Southern Queensland.
Analysis of piezoelectric solids with an efficient node-based element
Nguyen-Van, H., Mai-Duy, N. and Tran-Cong, T.. 2008. "Analysis of piezoelectric solids with an efficient node-based element." Schrefler, B. A. and Perego, U. (ed.) 8th World Congress on Computational Mechanics (WCCM8), and 5th European Congress on Computational Methods in Applied Sciences and Engineering (ECCOMAS 2008). Venice, Italy 30 Jun - 04 Jul 2008 Barcelona, Spain.
An IRBFN cartesian grid method based on displacement-stress formulation for 2D elasticity problems
Le, P., Mai-Duy, N., Tran-Cong, T. and Baker, G.. 2008. "An IRBFN cartesian grid method based on displacement-stress formulation for 2D elasticity problems." Schrefler, B. A. and Perego, U. (ed.) 8th World Congress on Computational Mechanics (WCCM8), and 5th European Congress on Computational Methods in Applied Sciences and Engineering (ECCOMAS 2008). Venice, Italy 30 Jun - 04 Jul 2008 Barcelona, Spain.
Solving 2D biharmonic equations by the Galerkin approach using integrated radial basis function networks
Mai-Duy, N. and Tran-Cong, T.. 2008. "Solving 2D biharmonic equations by the Galerkin approach using integrated radial basis function networks." Vigo-Aguiar, J., Khanal, H., Garcia Guirao, I. J., Oharu, S. and Venturino, E. (ed.) 8th International Conference on Computational and Mathematical Methods in Science and Engineering (CMMSE-2008). Murcia, Spain 13 - 17 Jun 2008 Murcia, Spain.
RBF interpolation of boundary values in the BEM for heat transfer problems
Mai-Duy, Nam and Tran-Cong, Thanh. 2003. "RBF interpolation of boundary values in the BEM for heat transfer problems." International Journal of Numerical Methods for Heat and Fluid Flow. 13 (5/6), pp. 611-632. https://doi.org/10.1108/09615530310482472
A meshless IRBFN-based method for transient problems
Mai-Cao, L. and Tran-Cong, T.. 2005. "A meshless IRBFN-based method for transient problems." CMES Computer Modeling in Engineering and Sciences. 7 (2), pp. 149-171.
An efficient indirect RBFN-based method for numerical solution of PDEs
Mai-Duy, Nam and Tran-Cong, Thanh. 2005. "An efficient indirect RBFN-based method for numerical solution of PDEs." Numerical Methods for Partial Differential Equations. 21 (4), pp. 770-790. https://doi.org/10.1002/num.20062
An effective RBFN-boundary integral approach for the analysis of natural convection flow
Mai-Duy, Nam and Tran-Cong, Thanh. 2004. "An effective RBFN-boundary integral approach for the analysis of natural convection flow." International Journal for Numerical Methods in Fluids. 46 (5), pp. 545-568. https://doi.org/10.1002/fld.769
Numerical solution of Navier-Stokes equations using multiquadric radial basis function networks
Mai-Duy, Nam and Tran-Cong, Thanh. 2001. "Numerical solution of Navier-Stokes equations using multiquadric radial basis function networks." International Journal for Numerical Methods in Fluids. 37 (1), pp. 65-86. https://doi.org/10.1002/fld.165
Numerical solution of differential equations using multiquadric radial basis function networks
Mai-Duy, Nam and Tran-Cong, Thanh. 2001. "Numerical solution of differential equations using multiquadric radial basis function networks." Neural Networks. 14 (2), pp. 185-199. https://doi.org/10.1016/S0893-6080(00)00095-2
Approximation of function and its derivatives using radial basis function networks
Mai-Duy, Nam and Tran-Cong, Thanh. 2003. "Approximation of function and its derivatives using radial basis function networks." Applied Mathematical Modelling: simulation and computation for engineering and environmental systems. 27 (3), pp. 197-220. https://doi.org/10.1016/S0307-904X(02)00101-4
A new meshless RBF-based method for unsteady fluid flow analysis
Mai-Duy, N., Mai-Cao, L. and Tran-Cong, T.. 2006. "A new meshless RBF-based method for unsteady fluid flow analysis." Sladek, Jan and Sladek, Vladimir (ed.) Advances in meshless methods. USA. Tech Science Press. pp. 241-262
A domain-type boundary-integral-equation method for two-dimensional biharmonic Dirichlet problem
Mai-Duy, N., Tran-Cong, T. and Tanner, R. I.. 2006. "A domain-type boundary-integral-equation method for two-dimensional biharmonic Dirichlet problem." Engineering Analysis with Boundary Elements. 30 (10), pp. 809-817. https://doi.org/10.1016/j.enganabound.2006.06.002
Meshfree direct and indirect local radial basis function collocation formulations for transport phenomena
Sarler, Bozidar, Tran-Cong, Thanh and Chen, Ching S.. 2005. "Meshfree direct and indirect local radial basis function collocation formulations for transport phenomena." Kassab, Alain J., Brebbia, Carlos Alberto, Divo, E. and Poljak, Dragan (ed.) 27th World Conference on Boundary Elements and Other Mesh reduction Methods Incorporating Engineering and Electromagnetics (BEM XXVII). Orlando, United States 15 - 18 Mar 2005 Southampton, United Kingdom.
Modeling and influence of shear retention parameter on the response of reinforced concrete structural elements
Dahmani, L., Khennane, A. and Kaci, S.. 2009. "Modeling and influence of shear retention parameter on the response of reinforced concrete structural elements." Strength of Materials. 41 (4), pp. 423-430. https://doi.org/10.1007/s11223-009-9139-y
Spinning CNT based composite yarns using a dry spinning process
Tran, Canh-Dung, Smith, Shaun M., Higgerson, G., Bui, Anh, Randeniya, Lakshman K. and Tran-Cong, Thanh. 2010. "Spinning CNT based composite yarns using a dry spinning process." Dzurak, Andrew (ed.) 2010 International Conference on Nanoscience and Nanotechnology (ICONN 2010). Sydney, Australia 22 - 26 Feb 2010 Piscataway, NJ. United States. https://doi.org/10.1109/ICONN.2010.6045159
Compact local integrated-RBF approximations for second-order elliptic differential problems
Mai-Duy, N. and Tran-Cong, T.. 2011. "Compact local integrated-RBF approximations for second-order elliptic differential problems." Journal of Computational Physics. 230 (12), pp. 4772-4794. https://doi.org/10.1016/j.jcp.2011.03.002
Element-free simulation of dilute polymeric flows using Brownian configuration fields
Tran, Canh-Dung and Tran-Cong, Thanh. 2004. "Element-free simulation of dilute polymeric flows using Brownian configuration fields." Korea-Australia Rheology Journal. 16 (1), pp. 1-15.
Kinetics of in situ epoxidation of hemp oil under heterogeneous reaction conditions: an overview with preliminary results
Cooney, T. I., Cardona, F. and Tran-Cong, T.. 2011. "Kinetics of in situ epoxidation of hemp oil under heterogeneous reaction conditions: an overview with preliminary results." Cowled, Craig J. L. (ed.) 1st International Postgraduate Conference on Engineering, Designing and Developing the Built Environment for Sustainable Wellbeing (eddBE 2011). Brisbane, Australia 27 - 29 Apr 2011 Brisbane, Australia.
A simple and effective preconditioner for integrated-RBF-based Cartesian-grid schemes
Mai-Duy, Nam and Tran-Cong, Thanh. 2010. "A simple and effective preconditioner for integrated-RBF-based Cartesian-grid schemes." Pepper, D. W. and Atluri, Satya N. (ed.) 2010 International Conference on Computational and Experimental Engineering & Sciences 2010. Las Vegas, United States of America 28 Mar - 01 Apr 2010 USA. https://doi.org/10.3970/icces.2010.014.051
Computation of viscoelastic flow using neural networks and stochastic simulation
Tran, Canh-Dung and Tran-Cong, Thanh. 2002. "Computation of viscoelastic flow using neural networks and stochastic simulation." Korea-Australia Rheology Journal. 14 (4), pp. 161-174.
BEM-NN computation of generalised Newtonian flows
Tran, Canh-D. and Tran-Cong, T.. 2002. "BEM-NN computation of generalised Newtonian flows." Engineering Analysis with Boundary Elements. 26 (1), pp. 15-28. https://doi.org/10.1016/S0955-7997(01)00085-6
Computation of dilute polymer solution flows using BCF-RBFN based method and domain decomposition technique
Tran, Canh-Dung, Phillips, David G. and Tran-Cong, Thanh. 2009. "Computation of dilute polymer solution flows using BCF-RBFN based method and domain decomposition technique." Korea-Australia Rheology Journal. 21 (1), pp. 1-12.
Towards an analysis of shear suspension flows using radial basis functions
Le-Cao, K., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2010. "Towards an analysis of shear suspension flows using radial basis functions." CMES Computer Modeling in Engineering and Sciences. 67 (3), pp. 265-294. https://doi.org/10.3970/cmes.2010.067.265
A new integrated-RBF-based domain-embedding scheme for solving fluid-flow problems
Le-Cao, K., Mai-Duy, N., Tran, C.-D. and Tran-Cong, T.. 2010. "A new integrated-RBF-based domain-embedding scheme for solving fluid-flow problems." Khalili, N., Valliappan, S., Li, Q. and Russell, A. (ed.) 9th World Congress on Computational Mechanics and 4th Asian-Pacific Congress on Computational Mechanics (WCCM/APCOM 2010). Sydney, Australia 19 - 23 Jul 2010 United Kingdom. IOP Publishing. https://doi.org/10.1088/1757-899X/10/1/012021
Galerkin/collocation methods based on 1D-integrated-RBFNs for viscoelastic flows
Ho-Minh, D., Mai-Duy, Nam and Tran-Cong, Thanh. 2010. "Galerkin/collocation methods based on 1D-integrated-RBFNs for viscoelastic flows." CMES Computer Modeling in Engineering and Sciences. 70 (3), pp. 217-251. https://doi.org/10.3970/cmes.2010.070.217
A Cartesian-grid integrated-RBF Galerkin technique
Ho-Minh, D., Mai-Duy, N. and Tran-Cong, T.. 2010. "A Cartesian-grid integrated-RBF Galerkin technique." Sarler, Bozidar and Atluri, Satya N. (ed.) Recent studies in meshless and other novel computational methods. Duluth, GA. USA. Tech Science Press. pp. 87-102
A numerical scheme based on local integrated RBFNs and Cartesian grids for solving second-order elliptic problems in two dimensions
Mai-Duy, N. and Tran-Cong, T.. 2010. "A numerical scheme based on local integrated RBFNs and Cartesian grids for solving second-order elliptic problems in two dimensions." Sarler, Bozidar and Atluri, Satya N. (ed.) Recent studies in meshless and other novel computational methods. Duluth, GA. United States. Tech Science Press. pp. 17-33
A numerical study of 2D integrated RBFNs incorporating Cartesian grids for solving 2D elliptic differential problems
Mai-Duy, Nam and Tran-Cong, Thanh. 2010. "A numerical study of 2D integrated RBFNs incorporating Cartesian grids for solving 2D elliptic differential problems." Numerical Methods for Partial Differential Equations. 26 (6), pp. 1443-1462. https://doi.org/10.1002/num.20502
A moving IRBFN-based integration-free meshless method
Le, Phong B. H., Rabczuk, Timon, Mai-Duy, Nam and Tran-Cong, Thanh. 2010. "A moving IRBFN-based integration-free meshless method." CMES Computer Modeling in Engineering and Sciences. 61 (1), pp. 63-109. https://doi.org/10.3970/cmes.2010.061.063
A moving IRBFN-based Galerkin meshless method
Le, Phong B. H., Rabczuk, Timon, Mai-Duy, Nam and Tran-Cong, Thanh. 2010. "A moving IRBFN-based Galerkin meshless method." CMES Computer Modeling in Engineering and Sciences. 66 (1), pp. 25-52. https://doi.org/10.3970/cmes.2010.066.025
A control volume technique based on integrated RBFNs for the convection-diffusion equation
Mai-Duy, Nam and Tran-Cong, Thanh. 2010. "A control volume technique based on integrated RBFNs for the convection-diffusion equation." Numerical Methods for Partial Differential Equations. 26 (2), pp. 426 -447. https://doi.org/10.1002/num.20444
A cartesian-grid collocation technique with integrated radial basis functions for mixed boundary value problems
Le, Phong B. H., Mai-Duy, Nam, Tran-Cong, Thanh and Baker, Graham. 2010. "A cartesian-grid collocation technique with integrated radial basis functions for mixed boundary value problems." International Journal for Numerical Methods in Engineering. 82 (4), pp. 435-463. https://doi.org/10.1002/nme.2771
Simulation of fluid flows at high Reynolds/Rayleigh numbers using integrated radial basis functions
Ho-Minh, D., Le-Cao, K., Mai-Duy, N. and Tran-Cong, T.. 2010. "Simulation of fluid flows at high Reynolds/Rayleigh numbers using integrated radial basis functions." Mallinson, G. D. and Cater, J. E. (ed.) 17th Australasian Fluid Mechanics Conference (AFMC 2010). Auckland, New Zealand 05 - 09 Dec 2010 Auckland, New Zealand.
Point-wise integrated-RBF-based discretisation of differential equations
Mai-Duy, Nam and Tran-Cong, Thanh. 2010. "Point-wise integrated-RBF-based discretisation of differential equations." Lu, Jane Wei-Zhen, Leung, Andrew Y. T., Lu, Vai Pan and Mok, Kai Meng (ed.) 2nd International Symposium on Computational Mechanics (ISCM II) in conjunction with EPMESC 2009. Hong Kong, China 30 Nov - 03 Dec 2009 College Park, MD. United States. AIP Publishing. https://doi.org/10.1063/1.3452151
A cartesian-grid integrated-RBF method for viscoelastic flows
Ho-Minh, D., Mai-Duy, N. and Tran-Cong, T.. 2010. "A cartesian-grid integrated-RBF method for viscoelastic flows." Khalili, N., Valliappan, S., Li, Q. and Russell, A. (ed.) 9th World Congress on Computational Mechanics and 4th Asian-Pacific Congress on Computational Mechanics (WCCM/APCOM 2010). Sydney, Australia 19 - 23 Jul 2010 Bristol, United Kingdom. IOP Publishing. https://doi.org/10.1088/1757-899X/10/1/012210
An upwind control-volume method based on integrated RBFs for fluid-flow problems
Mai-Duy, N. and Tran-Cong, T.. 2010. "An upwind control-volume method based on integrated RBFs for fluid-flow problems." Khalili, N., Valliappan, S., Li, Q. and Russell, A. (ed.) 9th World Congress on Computational Mechanics and 4th Asian-Pacific Congress on Computational Mechanics (WCCM/APCOM 2010). Sydney, Australia 19 - 23 Jul 2010 Bristol, United Kingdom. IOP Publishing. https://doi.org/10.1088/1757-899X/10/1/012023
Integrated-RBF network method for free vibration analysis of laminated composite plates
Ngo-Cong, D., Mai-Duy, N., Karunasena, W. and Tran-Cong, T.. 2010. "Integrated-RBF network method for free vibration analysis of laminated composite plates." Khalili, N., Valliappan, S., Li, Q. and Russell, A. (ed.) 9th World Congress on Computational Mechanics and 4th Asian-Pacific Congress on Computational Mechanics (WCCM/APCOM 2010). Sydney, Australia 19 - 23 Jul 2010 Bristol, United Kingdom. IOP Publishing. https://doi.org/10.1088/1757-899X/10/1/012236
A Cartesian-grid discretisation scheme based on local integrated RBFNs for two-dimensional elliptic problems
Mai-Duy, Nam and Tran-Cong, Thanh. 2009. "A Cartesian-grid discretisation scheme based on local integrated RBFNs for two-dimensional elliptic problems." CMES Computer Modeling in Engineering and Sciences. 51 (3), pp. 213-238. https://doi.org/10.3970/cmes.2009.051.213
On the use of integrated radial basis function schemes in weighted residuals statements for elliptic problems
Mai-Duy, Nam and Tran-Cong, Thanh. 2009. "On the use of integrated radial basis function schemes in weighted residuals statements for elliptic problems." Brebbia, Carlos A. (ed.) 31st International Conference on Boundary Elements and Other Mesh Reduction Methods (BEM/MRM 31). New Forest, United Kingdom 02 - 04 Sep 2009 Southampton, United Kingdom. https://doi.org/10.2495/BE090161
An improved quadrilateral flat element with drilling degrees of freedom for shell structural analysis
Nguyen-Van, Hieu, Mai-Duy, Nam and Tran-Cong, Thanh. 2009. "An improved quadrilateral flat element with drilling degrees of freedom for shell structural analysis." CMES Computer Modeling in Engineering and Sciences. 49 (2), pp. 81-110. https://doi.org/10.3970/cmes.2009.049.081
Integrated radial-basis-function networks for computing Newtonian and non-Newtonian fluid flows
Mai-Duy, Nam and Tran-Cong, Thanh. 2009. "Integrated radial-basis-function networks for computing Newtonian and non-Newtonian fluid flows." Computers and Structures. 87 (11-12), pp. 642-650. https://doi.org/10.1016/j.compstruc.2008.09.004
Energy analysis of hydraulic fracturing
Golshani, Aliakbar and Tran-Cong, Thanh. 2009. "Energy analysis of hydraulic fracturing." KSCE Journal of Civil Engineering. 13 (4), pp. 219-224. https://doi.org/10.1007/s12205-009-0219-0
An effective integrated-RBFN Cartesian-grid discretization for the stream function-vorticity-temperature formulation in nonrectangular domains
Le-Cao, K., Mai-Duy, N. and Tran-Cong, T.. 2009. "An effective integrated-RBFN Cartesian-grid discretization for the stream function-vorticity-temperature formulation in nonrectangular domains." Numerical Heat Transfer Part B: Fundamentals. 55 (6), pp. 480-502. https://doi.org/10.1080/10407790902827470
An integrated-RBF technique based on Galerkin formulation for elliptic differential equations
Mai-Duy, Nam and Tran-Cong, Thanh. 2009. "An integrated-RBF technique based on Galerkin formulation for elliptic differential equations." Engineering Analysis with Boundary Elements. 33 (2), pp. 191-199. https://doi.org/10.1016/j.enganabound.2008.05.001
A Galerkin-RBF approach for the streamfunction-vorticity-temperature formulation of natural convection in 2D enclosured domains
Ho-Minh, D., Mai-Duy, Nam and Tran-Cong, Thanh. 2009. "A Galerkin-RBF approach for the streamfunction-vorticity-temperature formulation of natural convection in 2D enclosured domains." CMES Computer Modeling in Engineering and Sciences. 44 (3), pp. 219-248. https://doi.org/10.3970/cmes.2009.044.219
A spectral collocation technique based on integrated Chebyshev polynomials for biharmonic problems in irregular domains
Mai-Duy, Nam, See, Howard and Tran-Cong, Thanh. 2009. "A spectral collocation technique based on integrated Chebyshev polynomials for biharmonic problems in irregular domains." Applied Mathematical Modelling: simulation and computation for engineering and environmental systems. 33 (1), pp. 284-299. https://doi.org/10.1016/j.apm.2007.11.002
A Galerkin approach incorporating integrated radial basis function networks for the solution of 2D biharmonic equations
Mai-Duy, Nam, Ho-Minh, D. and Tran-Cong, Thanh. 2009. "A Galerkin approach incorporating integrated radial basis function networks for the solution of 2D biharmonic equations." International Journal of Computer Mathematics. 86 (10-11), pp. 1746-1759. https://doi.org/10.1080/00207160802647365
Investigation of a hydraulic impact: a technology in rock breaking
Genet, Martin, Yan, Wenyi and Tran-Cong, Thanh. 2009. "Investigation of a hydraulic impact: a technology in rock breaking." Archive of Applied Mechanics. 79 (9), pp. 825-841. https://doi.org/10.1007/s00419-008-0256-z
Automated carbon dioxide measurement via miniaturised chemical reaction chambers under mechatronic control
Maxwell, Andrew, Hancock, Nigel and Tran-Cong, Thanh. 2000. "Automated carbon dioxide measurement via miniaturised chemical reaction chambers under mechatronic control." Billingsley, John (ed.) Mechatronics and machine vision. Baldock, United Kingdom. Research Studies Press. pp. 135-142
A meshless technique based on integrated radial basis function networks for elliptic partial differential equations
Mai-Duy, N. and Tran-Cong, T.. 2008. "A meshless technique based on integrated radial basis function networks for elliptic partial differential equations." Griebel, Michael and Schweitzer, Marc Alexander (ed.) 4th International Workshop on Meshfree Methods for Partial Differential Equations. Bonn, Germany 17 - 20 Sep 2007 Berlin, Germany. https://doi.org/10.1007/978-3-540-79994-8_9
On the use of integrated RBFs in Galerkin approximation for elliptic problems
Mai-Duy, Nam and Tran-Cong, Thanh. 2008. "On the use of integrated RBFs in Galerkin approximation for elliptic problems." Skerget, Leopold and Brebbia, Carlos A. (ed.) BEM/MRM 30: 30th International Conference on Boundary Elements and Other Mesh Reduction Methods. Maribor, Slovenia 07 - 09 Jul 2008 Southampton, United Kingdom. https://doi.org/10.2495/BE080171
An effective high-order point-collocation numerical approach based on integrated approximants for elliptic differential equations
Mai-Duy, N. and Tran-Cong, T.. 2008. "An effective high-order point-collocation numerical approach based on integrated approximants for elliptic differential equations." Alvarez, Matias P. (ed.) Leading-edge applied mathematical modeling research. New York, NY. United States. Nova Science Publishers. pp. 215-250
A multidomain integrated-radial-basis-function collocation method for elliptic problems
Mai-Duy, Nam and Tran-Cong, Thanh. 2008. "A multidomain integrated-radial-basis-function collocation method for elliptic problems." Numerical Methods for Partial Differential Equations. 24 (5), pp. 1301-1320. https://doi.org/10.1002/num.20319
Free vibration analysis of laminated plate/shell structures based on FSDT with a stabilized nodal-integrated quadrilateral element
Nguyen-Van, H., Mai-Duy, N. and Tran-Cong, T.. 2008. "Free vibration analysis of laminated plate/shell structures based on FSDT with a stabilized nodal-integrated quadrilateral element." Journal of Sound and Vibration. 313 (1-2), pp. 205-223. https://doi.org/10.1016/j.jsv.2007.11.043
Nodal integration finite element techniques for analysis of piezoelectric solids
Nguyen-Van, Hieu, Le, Thong, Mai-Duy, Nam and Tran-Cong, Thanh. 2008. "Nodal integration finite element techniques for analysis of piezoelectric solids." 2008 International Conference on Computational Solid Mechanics (CSM2008). Ho Chi Minh City, Vietnam 27 - 30 Nov 2008 Ho Chi Minh City, Vietnam.
Simulation of hydraulic fracturing in brittle rocks
Golshani, Aliakbar and Tran-Cong, Thanh. 2008. "Simulation of hydraulic fracturing in brittle rocks." Majdi, Abass and Ghazvinian, Abdolhadi (ed.) ISRM International Symposium 2008: 5th Asian Rock Mechanics Symposium. Tehran, Iran 24 - 26 Nov 2008 Iran.
An integral-collocation-based fictitious-domain technique for solving elliptic problems
Mai-Duy, Nam, See, Howard and Tran-Cong, Thanh. 2008. "An integral-collocation-based fictitious-domain technique for solving elliptic problems." Communications in Numerical Methods in Engineering. 24 (11), pp. 1291-1314. https://doi.org/10.1002/cnm.1033
A point-collocation method based on integrated Chebyshev polynomials for elliptic differential equations in irregular domains
Mai-Duy, N. and Tran-Cong, T.. 2008. "A point-collocation method based on integrated Chebyshev polynomials for elliptic differential equations in irregular domains." Schrefler, B. A. and Perego, U. (ed.) 8th World Congress on Computational Mechanics (WCCM8), and 5th European Congress on Computational Methods in Applied Sciences and Engineering (ECCOMAS 2008). Venice, Italy 30 Jun - 04 Jul 2008 Barcelona, Spain.
A multidomain integrated RBF collocation method for elliptic differential equations
Mai-Duy, Nam and Tran-Cong, Thanh. 2008. "A multidomain integrated RBF collocation method for elliptic differential equations." Schrefler, B. A. and Perego, U. (ed.) 8th World Congress on Computational Mechanics (WCCM8), and 5th European Congress on Computational Methods in Applied Sciences and Engineering (ECCOMAS 2008). Venice, Italy 30 Jun - 04 Jul 2008 Barcelona, Spain.
An efficient domain-decomposition pseudo-spectral method for solving elliptic differential equations
Mai-Duy, Nam and Tran-Cong, Thanh. 2008. "An efficient domain-decomposition pseudo-spectral method for solving elliptic differential equations." Communications in Numerical Methods in Engineering. 24 (10), pp. 795-806. https://doi.org/10.1002/cnm.987
A node-based element for analysis of planar piezoelectric structures
Nguyen-Van, Hieu, Mai-Duy, Nam and Tran-Cong, Thanh. 2008. "A node-based element for analysis of planar piezoelectric structures." CMES Computer Modeling in Engineering and Sciences. 36 (1), pp. 65-95. https://doi.org/10.3970/cmes.2008.036.065
A meshless modeling of dynamic strain localization in quasi-brittle materials using radial basis function networks
Le, P., Mai-Duy, N., Tran-Cong, T. and Baker, G.. 2008. "A meshless modeling of dynamic strain localization in quasi-brittle materials using radial basis function networks." CMES Computer Modeling in Engineering and Sciences. 25 (1), pp. 43-67. https://doi.org/10.3970/cmes.2008.025.043
A second-order continuity domain-decomposition technique based on integrated Chebyshev polynomials for two-dimensional elliptic problems
Mai-Duy, Nam and Tran-Cong, Thanh. 2008. "A second-order continuity domain-decomposition technique based on integrated Chebyshev polynomials for two-dimensional elliptic problems." Applied Mathematical Modelling: simulation and computation for engineering and environmental systems. 32 (12), pp. 2851-2862. https://doi.org/10.1016/j.apm.2007.10.003
Energy analysis of hydraulic fracturing
Golshani, Aliakbar and Tran-Cong, Thanh. 2008. "Energy analysis of hydraulic fracturing." Singh, D. N., Carter, J., Desai, C. S., Dolezalova, M., Gioda, G., Madhav, M. R., Oka, F., Vanapalli, S., Yin, J. H. and Zaman, M. M. (ed.) 12th International Conference of IACMAG. Goa, India 01 - 06 Oct 2008 India.
A smoothed four-node piezoelectric element for analysis of two-dimensional smart structures
Nguyen-Van, Hieu, Mai-Duy, Nam and Tran-Cong, Thanh. 2008. "A smoothed four-node piezoelectric element for analysis of two-dimensional smart structures." CMES Computer Modeling in Engineering and Sciences. 23 (3), pp. 209-222. https://doi.org/10.3970/cmes.2008.023.209
A meshless approach to capturing moving interfaces in passive transport problems
Mai-Cao, L. and Tran-Cong, T.. 2008. "A meshless approach to capturing moving interfaces in passive transport problems." CMES Computer Modeling in Engineering and Sciences. 31 (3), pp. 157-188. https://doi.org/10.3970/cmes.2008.031.157
Impact on a water filled cylinder
Golshani, Aliakbar, Tran-Cong, Thanh and Buttsworth, David. 2008. "Impact on a water filled cylinder." Ashida, Fumihiro and Sakata, Sei-ichiro (ed.) ACMFMS 2008: Asian Conference on Mechanics of Functional Materials and Structures. Matsue, Japan 31 Oct - 03 Nov 2008 Japan.
A Cartesian grid technique based on one-dimensional integrated radial basis function networks for natural convection in concentric annuli
Mai-Duy, Nam, Le-Cao, Khoa and Tran-Cong, Thanh. 2008. "A Cartesian grid technique based on one-dimensional integrated radial basis function networks for natural convection in concentric annuli." International Journal for Numerical Methods in Fluids. 57 (12), pp. 1709-1730. https://doi.org/10.1002/fld.1675
A RBF-based fictitious-domain technique for Dirichlet boundary value problems in multiply-connected domains
Mai-Duy, Nam and Tran-Cong, Thanh. 2007. "A RBF-based fictitious-domain technique for Dirichlet boundary value problems in multiply-connected domains." Yagawa, G., Iu, V. P., Kashiyama, K., Miyazaki, N., Arantes e Oliveira, E., Valliappan, S., Yabe, T. and Yuan, M. W. (ed.) 3rd Asian-Pacific Congress on Computational Mechanics (APCOM'07) and EPMESC XI. Kyoto, Japan 03 - 06 Dec 2007 Japan.
A meshless IRBFN-based numerical simulation of dynamic strain localization in quasi-brittle materials
Le, Phong, Mai-Duy, Nam, Tran-Cong, Thanh and Baker, Graham. 2007. "A meshless IRBFN-based numerical simulation of dynamic strain localization in quasi-brittle materials." Taylor, R. L., Papadopoulos, P. and Zohdi, T. I. (ed.) USNCCM9: 9th US National Congress on Computational Mechanics. San Francisco, United States 22 - 26 Jul 2007 Austin, TX. United States.
Timoshenko beam-solution in terms of integrated radial basis functions
Khennane, Amar and Tran-Cong, Thanh. 2007. "Timoshenko beam-solution in terms of integrated radial basis functions." Veidt, Martin, Albermani, Faris, Daniel, Bill, Griffiths, John, Hargreaves, Doug, McAree, Ross, Meehan, Paul and Tan, Andy (ed.) 5th Australasian Congress on Applied Mechanics (ACAM 2007). Brisbane, Australia 10 - 12 Dec 2007 Sydney, Australia.
Solving partial differential equations with point collocation and one-dimensional integrated interpolation schemes
Mai-Duy, Nam and Tran-Cong, Thanh. 2007. "Solving partial differential equations with point collocation and one-dimensional integrated interpolation schemes." Han, Z., Lee, S. W. and Nakagaki, M. (ed.) 14th International Conference on Computational & Experimental Engineering and Sciences. Miami, Florida, USA 01 - 03 Jan 2007 United States.
Computation of laminated composite plates using integrated radial basis function networks
Mai-Duy, Nam, Khennane, Amar and Tran-Cong, Thanh. 2007. "Computation of laminated composite plates using integrated radial basis function networks." Computers, Materials and Continua. 5 (1), pp. 63-77. https://doi.org/10.3970/cmc.2007.005.063
A numerical study of strain localization in elasto-thermo-viscoplastic materials using radial basis function networks
Le, Phong, Mai-Duy, Nam, Tran-Cong, Thanh and Baker, Graham. 2007. "A numerical study of strain localization in elasto-thermo-viscoplastic materials using radial basis function networks." Computers, Materials and Continua. 5 (2), pp. 129-150. https://doi.org/10.3970/cmc.2007.005.129
A simple and accurate four-node quadrilateral element using stabilized nodal integration for laminated plates
Nguyen-Van, Hieu, Mai-Duy, Nam and Tran-Cong, Thanh. 2007. "A simple and accurate four-node quadrilateral element using stabilized nodal integration for laminated plates." Computers, Materials and Continua. 6 (3), pp. 159-176. https://doi.org/10.3970/cmc.2007.006.159
Computation of transient viscous flows using indirect radial basis function networks
Mai-Duy, Nam, Mai-Cao, Lan and Tran-Cong, Thanh. 2007. "Computation of transient viscous flows using indirect radial basis function networks." CMES Computer Modeling in Engineering and Sciences. 18 (1), pp. 59-78. https://doi.org/10.3970/cmes.2007.018.059
A Cartesian-grid collocation method based on radial-basis-function networks for solving PDEs in irregular domains
Mai-Duy, Nam and Tran-Cong, Thanh. 2007. "A Cartesian-grid collocation method based on radial-basis-function networks for solving PDEs in irregular domains." Numerical Methods for Partial Differential Equations. 23 (5), pp. 1192-1210. https://doi.org/10.1002/num.20217
Analysis of laminated composite plate/shell structures using a stabilized nodal-integrated quadrilateral element
Nguyen-Van, Hieu, Mai-Duy, Nam and Tran-Cong, Thanh. 2007. "Analysis of laminated composite plate/shell structures using a stabilized nodal-integrated quadrilateral element." Mendis, P. A., Cao, D. T. and Ngo, T. (ed.) 1st International Conference on Modern Design, Construction & Maintenance of Structures. Hanoi, Vietnam 10 - 11 Dec 2007 Hanoi, Vietnam.
Analysis of viscoelastic flow by a radial basis function networks method
Ho-Minh, D., Mai-Duy, Nam and Tran-Cong, Thanh. 2007. "Analysis of viscoelastic flow by a radial basis function networks method." Jacobs, Peter A., McIntyre, Tim, Cleary, Matthew J., Buttsworth, David R., Mee, David, Clements, Rose, Morgan, Richard and Lemckert, Charles (ed.) 16th Australasian Fluid Mechanics Conference (AFMC 2007). Gold Coast, Australia 03 - 07 Dec 2007 Brisbane, Australia.
Radial-basis-function calculations of buoyancy-driven flow in concentric and eccentric annuli
Le-Cao, Khoa, Mai-Duy, Nam and Tran-Cong, Thanh. 2007. "Radial-basis-function calculations of buoyancy-driven flow in concentric and eccentric annuli." Jacobs, Peter A., McIntyre, Tim, Cleary, Matthew J., Buttsworth, David R., Mee, David, Clements, Rose, Morgan, Richard and Lemckert, Charles (ed.) 16th Australasian Fluid Mechanics Conference (AFMC 2007). Gold Coast, Australia 03 - 07 Dec 2007 Brisbane, Australia.
Boundary integral-based domain decomposition technique for solution of Navier Stokes equations
Mai-Duy, N. and Tran-Cong, T.. 2004. "Boundary integral-based domain decomposition technique for solution of Navier Stokes equations." CMES Computer Modeling in Engineering and Sciences. 6 (1), pp. 59-75. https://doi.org/10.3970/cmes.2004.006.059
Indirect RBFN method with thin plate splines for numerical solution of differential equations
Mai-Duy, N. and Tran-Cong, T.. 2003. "Indirect RBFN method with thin plate splines for numerical solution of differential equations." CMES Computer Modeling in Engineering and Sciences. 4 (1), pp. 85-102. https://doi.org/10.3970/cmes.2003.004.085
A micromechanics model for environmental stress-corrosion in GFRP
Khennane, Amar and Melchers, Robert E.. 2003. "A micromechanics model for environmental stress-corrosion in GFRP." International Journal of Materials and Product Technology. 19 (1), pp. 2-14. https://doi.org/10.1504/IJMPT.2003.003556
Durability of glass polymer composites subject to stress corrosion
Khennane, Amar and Melchers, Robert E.. 2003. "Durability of glass polymer composites subject to stress corrosion." Journal of Composites for Construction. 7 (2), pp. 109-117. https://doi.org/10.1061/(ASCE)1090-0268(2003)7:2(109)
Stress corrosion of glass fibre reinforced polymers for infrastructure applications
Khennane, Amar and Melchers, Robert. 2002. "Stress corrosion of glass fibre reinforced polymers for infrastructure applications." 41st Australasian Corrosion Association Inc Conference (ACA 2001): Corrosion and Prevention. Newcastle, Australia 18 - 21 Nov 2001 Melbourne, Australia.
BEM-RBF approach for viscoelastic flow analysis
Tran-Cong, T., Mai-Duy, N. and Phan-Thien, N.. 2002. "BEM-RBF approach for viscoelastic flow analysis." Engineering Analysis with Boundary Elements. 26 (9), pp. 757-762. https://doi.org/10.1016/S0955-7997(02)00041-3
Mesh-free radial basis function network methods with domain decomposition for approximation of functions and numerical solution of Poisson's equations
Mai-Duy, Nam and Tran-Cong, Thanh. 2002. "Mesh-free radial basis function network methods with domain decomposition for approximation of functions and numerical solution of Poisson's equations." Engineering Analysis with Boundary Elements. 26 (2), pp. 133-156. https://doi.org/10.1016/S0955-7997(01)00092-3
A fast convergent iterative boundary element method on PVM cluster
Mai-Duy, N., Nguyen-Hong, P. and Tran-Cong, T.. 1998. "A fast convergent iterative boundary element method on PVM cluster." Engineering Analysis with Boundary Elements. 22 (4), pp. 307-316. https://doi.org/10.1016/S0955-7997(98)00071-X
An improved boundary element method for analysis of profile polymer extrusion
Nguyen-Thien, T., Tran-Cong, T. and Phan-Thien, N.. 1997. "An improved boundary element method for analysis of profile polymer extrusion." Engineering Analysis with Boundary Elements. 20 (1), pp. 81-89.
BEM-RBF approach for viscoelastic flow analysis
Tran-Cong, T., Mai-Duy, N. and Phan-Thien, N.. 2001. "BEM-RBF approach for viscoelastic flow analysis." Beskos, D., Brebbia, C., Katsikadelis, J. and Manolis, G. (ed.) 23rd International Conference on the Boundary Element Method (BEM 2001). Lemnos, Greece 07 - 09 May 2001 Southampton, Hants. United Kingdom. https://doi.org/10.2495/BE010301
Non-contact extrudate profilometer: introductory paper
Taylor, Reginald, Hancock, Nigel and Tran-Cong, Thanh. 1997. "Non-contact extrudate profilometer: introductory paper." Werner, B. (ed.) 4th Annual Conference on Mechatronics and Machine Vision in Practice (MViP 1997). Toowoomba, Australia 23 - 25 Sep 1997 USA. https://doi.org/10.1109/MMVIP.1997.625315
Autonomous LHD loading
Petty, Matt K., Billingsley, John and Tran-Cong, Thanh. 1997. "Autonomous LHD loading." Werner, Bob (ed.) 4th Annual Conference on Mechatronics and Machine Vision in Practice (MViP 1997). Toowoomba, Australia 23 - 25 Sep 1997 Los Alamitos, CA. United States. https://doi.org/10.1109/MMVIP.1997.625330
A meshless level-set scheme for interfacial flows
Mai-Cao, L. and Tran-Cong, T.. 2006. "A meshless level-set scheme for interfacial flows." Nguyen, Son Q. and Nguyen, Dung (ed.) 2006 International Conference on Nonlinear Analysis & Engineering Mechanics Today. Ho Chi Minh City, Vietnam 11 - 14 Dec 2006 Paris, France.
Modelling a borehole subjected to fluid pressure
Golshani, Aliakbar and Tran-Cong, Thanh. 2006. "Modelling a borehole subjected to fluid pressure." Nguyen, Son Q. and Nguyen, Dung (ed.) 2006 International Conference on Nonlinear Analysis & Engineering Mechanics Today. Ho Chi Minh City, Vietnam 11 - 14 Dec 2006 Paris, France.
A meshless IRBFN-based numerical simulation of adiabatic shear band formation in one dimension
Le, Phong, Mai-Duy, Nam, Tran-Cong, Thanh and Baker, Graham. 2006. "A meshless IRBFN-based numerical simulation of adiabatic shear band formation in one dimension." Nguyen, Son Q. and Nguyen, Dung (ed.) 2006 International Conference on Nonlinear Analysis & Engineering Mechanics Today. Ho Chi Minh City, Vietnam 11 - 14 Dec 2006 Paris, France.
A high-order time-kernel BIEM for the Burgers equation
Mai-Duy, Nam, Tran-Cong, Thanh and Tanner, R. I.. 2006. "A high-order time-kernel BIEM for the Burgers equation." Gatmiri, B., Sellier, A. and Aliabadi, M. H. (ed.) International Conference on Boundary Element Techniques VII. Paris, France 04 - 06 Sep 2006 Eastleigh, United Kingdom.
A new high-order time-kernel BIEM for the Burgers equation
Mai-Duy, N., Tran-Cong, T. and Tanner, R. I.. 2006. "A new high-order time-kernel BIEM for the Burgers equation." CMES Computer Modeling in Engineering and Sciences. 16 (3), pp. 177-186. https://doi.org/10.3970/cmes.2006.016.177
Solving biharmonic problems with scattered-point discretization using indirect radial-basis-function networks
Mai-Duy, N. and Tran-Cong, T.. 2006. "Solving biharmonic problems with scattered-point discretization using indirect radial-basis-function networks." Engineering Analysis with Boundary Elements. 30 (2), pp. 77-87. https://doi.org/10.1016/j.enganabound.2005.10.004
Design and analysis of a composite beam for infrastructure applications - Part III: experimental results and nonlinear FE analysis
Springolo, Mario, Khennane, Amar and Van Erp, Gerard. 2006. "Design and analysis of a composite beam for infrastructure applications - Part III: experimental results and nonlinear FE analysis ." International Journal of Materials and Product Technology. 25 (4), pp. 331-347.
Design and analysis of a composite beam for infrastructure applications - Part II: preliminary investigation in shear and torsion
Springolo, Mario, Van Erp, Gerard and Khennane, Amar. 2006. "Design and analysis of a composite beam for infrastructure applications - Part II: preliminary investigation in shear and torsion ." International Journal of Materials and Product Technology. 25 (4), pp. 313-331.
Design and analysis of a composite beam for infrastructure applications - Part I: preliminary investigation in bending
Springolo, Mario, Van Erp, Gerard and Khennane, Amar. 2006. "Design and analysis of a composite beam for infrastructure applications - Part I: preliminary investigation in bending ." International Journal of Materials and Product Technology. 25 (4), pp. 297-313. https://doi.org/10.1504/IJMPT.2006.008885
Bounding the stability and rupture condition of emulsion and foam films
Coons, J., Halley, P., McGlashan, S. and Tran-Cong, T.. 2005. "Bounding the stability and rupture condition of emulsion and foam films." Chemical Engineering Research and Design. 83 (A7), pp. 915-925.
A meso-scale finite element model for environmental stress corrosion of GFRP
Khennane, Amar and Melchers, Robert E.. 2005. "A meso-scale finite element model for environmental stress corrosion of GFRP." Xie, Mike, Mouritz, Adrian, Khatibi, Akbar Afaghi, Gardiner, Craig and Chiu, Wing Kong (ed.) 4th Australasian Congress on Applied Mechanics (ACAM 2005). Melbourne, Australia 16 - 18 Feb 2005 Melbourne, Australia.
Performance design of reinforced concrete slabs using commercial finite element software
Khennane, Amar. 2005. "Performance design of reinforced concrete slabs using commercial finite element software." Structural Concrete. 6 (4), pp. 141-147.
Scaling laws for the critical rupture thickness of common thin films
Coons, J. E., Halley, P. J., McGlashan, S. A. and Tran-Cong, T.. 2005. "Scaling laws for the critical rupture thickness of common thin films." Colloids and Surfaces A: Physicochemical and Engineering Aspects. 263 (1-3), pp. 258-266. https://doi.org/10.1016/j.colsurfa.2005.01.008
Bounding film drainage in common thin films
Coons, J. E., Halley, P. J., McGlashan, S. A. and Tran-Cong, T.. 2005. "Bounding film drainage in common thin films." Colloids and Surfaces A: Physicochemical and Engineering Aspects. 263 (1-3), pp. 197-204. https://doi.org/10.1016/j.colsurfa.2005.01.009
Meso-scale finite element investigation into the short and long term strengths of glass fibre reinforced composites
Khennane, Amar and Melchers, Robert E.. 2003. Meso-scale finite element investigation into the short and long term strengths of glass fibre reinforced composites. Toowoomba, Australia. University of Southern Queensland.
Parallel meshfree TPSRBFN-BCF method for dilute polymer solution
Tran, CD and Tran-Cong, T.. 2003. "Parallel meshfree TPSRBFN-BCF method for dilute polymer solution." The 2nd Korean-Australian Rheology Conference 2003. Gyeongju , Korea 24 - 26 Sep 2003 Korea .
Comparison of BEM-FFNN and BEM-RBFN methods for GNF flow analysis
Tran, C., Mai-Duy, N. and Tran-Cong, T.. 2000. "Comparison of BEM-FFNN and BEM-RBFN methods for GNF flow analysis." The XIIIth International Congress on Rheology. Cambridge, United Kingdom 20 - 25 Aug 2000 United Kingdom.
Nonlinear analysis of reinforced concrete beams in a fire environment
Kaci, Salah, Sadaoui, Arezki and Khennane, Amar. 2003. "Nonlinear analysis of reinforced concrete beams in a fire environment." Ghobarah, Ahmed and Gould, Phillip (ed.) Response of Structures to Extreme Loading (2003). Toronto, Canada 03 - 06 Aug 2003 St. Louis, MO. United States.